Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Heat Seal Strength | 250 g/25 mm @Time 0.250 sec, Pressure 0.0345 MPa |
0.551 lb/in @Time 0.0000694 hour, Pressure 5.00 psi |
120°C, 35% RH |
DuPont Teijin Films Mylar® CL Polyester Film, 100 Gauge Mylar® CL is an exceptionally strong polyester film designed to package foods. Foods can be heated or cooked in this film at temperatures up to 400°F. Mylar® CL is commercially available in nomin.. |