Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Hot Tack Strength 700 g/25 mm
700 g/in
seal bar 115°C; Packforsk method.
DuPont Nucrel® 0609HS Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating  (discontinue
6 wt% Methacrylic Acid.Nucrel® 0609HS* (High-Speed) is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminatin..