Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hot Tack Strength | <= 2300 g/25 mm | <= 2300 g/in | Varies with seal bar temp.; Packforsk Method |
DuPont™ Surlyn® 1802 Sodium Ionomer Resin for Blown/Cast Film and Extrusion Coating Surlyn® 1802 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment and extrusion coating and coextrusion coating equipment designed to proces.. |