Polymer Property : Hot Tack Strength = 215 g/25 mm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Hot Tack Strength 215 g/25 mm
215 g/in
g/25 mm; Coating of 10 kg/ream; melt temp 325°C
NOVA Chemicals Sclair® 61C Octene LLDPE Extrusion Resin  (discontinued **)
Features: Octene co-polymer, excellent sealability and toughness, high drawdown, high adhesion, good barrier, good abrasion resistance.Applications: Food packaging, milk cartons, paperboard containe..