Mechanical Properties Metric English Comments
Hot Tack Strength 500 - 2000 g/25 mm
500 - 2000 g/in
Average value: 1030 g/25 mm Grade Count:8
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Coating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Coating Grade". Each property range of values reported is minimum an..