Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 88.1 J @Temperature -40.0 °C |
65.0 ft-lb @Temperature -40.0 °F |
0.144 in.; ARM test |
Polimeros Mexicanos Rotolene® 93835-TG Medium Density Polyethylene MDPE Copolymer with UV8 stabilizer in natural and colors.Recommended for rotomolding. Used for manufacture of water tanks > 2000 liters, cisterns, farm tanks, or tanks to contain strong acids and b.. |
|||
Impact Test | 88.1 J @Thickness 3.17 mm, Temperature -40.0 °C |
65.0 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
ARM impact |
A. Schulman SUPERLINEAR™ XL 0370 Rotational Molding Resin DescriptionSuperlinear XL 0370 is compounded rotational molding resin based on metallocean catalyst technology. This technology allows for high impact and excellent stiffness. It is typically used.. |
|||
Impact Test | 88.1 J @Thickness 3.17 mm, Temperature -40.0 °C |
65.0 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
ARM impact |
A. Schulman SUPERLINEAR™ XL 0370 Rotational Molding Resin DescriptionSuperlinear XL 0370 is compounded rotational molding resin based on metallocean catalyst technology. This technology allows for high impact and excellent stiffness. It is typically used.. |
|||
Impact Test | 88.1 J @Thickness 3.17 mm, Temperature -40.0 °C |
65.0 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
ARM impact |
A. Schulman SUPERLINEAR™ XL 0370 Rotational Molding Resin DescriptionSuperlinear XL 0370 is compounded rotational molding resin based on metallocean catalyst technology. This technology allows for high impact and excellent stiffness. It is typically used.. |
|||
Impact Test | 88.1 J @Thickness 3.17 mm, Temperature -40.0 °C |
65.0 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
ARM impact |
A. Schulman SUPERLINEAR™ XL 0370 Rotational Molding Resin DescriptionSuperlinear XL 0370 is compounded rotational molding resin based on metallocean catalyst technology. This technology allows for high impact and excellent stiffness. It is typically used.. |
|||
Impact Test | 88.1 J @Thickness 3.17 mm, Temperature -40.0 °C |
65.0 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
ARM impact |
A. Schulman SUPERLINEAR™ XL 0370 Rotational Molding Resin DescriptionSuperlinear XL 0370 is compounded rotational molding resin based on metallocean catalyst technology. This technology allows for high impact and excellent stiffness. It is typically used.. |
|||
Impact Test | 88.1 J @Thickness 3.17 mm, Temperature -40.0 °C |
65.0 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
ARM impact |
A. Schulman SUPERLINEAR™ XL 0370 Rotational Molding Resin DescriptionSuperlinear XL 0370 is compounded rotational molding resin based on metallocean catalyst technology. This technology allows for high impact and excellent stiffness. It is typically used.. |