Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 81.4 J @Temperature 23.0 °C |
60.0 ft-lb @Temperature 73.4 °F |
Instrumented Dart Total Energy |
Styron CALIBRE™ MEGARAD 2080 15 Polycarbonate, Gamma Radiation Resistant CALIBRE® MegaRad 2080 series resins provide end-users of radiation sterilized medical devices a color closer to the water-clear look of the natural resin. When exposed to high energy radiation (g.. |