Mechanical Properties Metric English Comments
Impact Test 7.91 J
5.83 ft-lb
Reverse; ASTM D2794
Chesterton ARC MX2 High Wear Fine Particle Wear Compound
Description: An advanced ceramic composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion and chemical attack. It is applied at a thickness of 3 mm (1/8”..