Mechanical Properties Metric English Comments
Impact Test 92.0 J
67.9 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Lexan® HFD1930 PC Copolymer
55 MFR LEXAN High Flow Ductile Copolymer, Natural color only
Impact Test 92.0 J
67.9 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Lexan® HFD1930 PC Copolymer (Asia Pacific)
55 MFR LEXAN High Flow Ductile Copolymer, Natural color only
Impact Test 92.0 J
67.9 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Lexan® HFD1930 PC Copolymer (Europe-Africa-Middle East)
55 MFR LEXAN High Flow Ductile Copolymer, Natural color only
Impact Test 92.0 J
67.9 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Lexan® HFD1910 PC Copolymer
55 MFR LEXAN High Flow Ductile Copolymer, Natural colors only
Impact Test 92.0 J
67.9 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Lexan® HFD1910 PC Copolymer (Asia Pacific)
55 MFR LEXAN High Flow Ductile Copolymer, Natural colors only
Impact Test 92.0 J
67.9 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Lexan® HFD1910 PC Copolymer (Europe-Africa-Middle East)
55 MFR LEXAN High Flow Ductile Copolymer, Natural colors only