Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 85.4 J | 63.0 ft-lb | Torque Strength; curing at 1000°F |
Aremco Ceramabond™ 835-M High Temperature Ceramic Adhesive/Paste, Alumina Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |