Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 5.76 J | 4.25 ft-lb | Reverse; ASTM D2794 |
Chesterton ARC BX2 Contractor Grade Fine Sliding Wear Compound Description: ARC BX2 is an advanced contractor grade ceramic reinforced composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It .. |