Mechanical Properties Metric English Comments
Impact Test 7.10 J
5.24 ft-lb
TUP Impact; 1" radius tip on 1/16" plaque
Ineos H28E-00 Polypropylene Homopolymer, Antistatic
Grade H28E-00 is an antistated, controlled rheology polypropylene homopolymer. It is designed for injection molding applications that require improved impact. This material meets the Food and Drug..