Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 64.0 J @Temperature 23.0 °C |
47.2 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Cycoloy® C3650 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according .. |
|||
Impact Test | 64.0 J @Temperature 23.0 °C |
47.2 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics Lexan® 105 PC General purpose low flow Polycarbonate powder gradeThis data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 64.0 J @Temperature 23.0 °C |
47.2 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics Lexan® 135 PC General purpose low flow polycarbonate powder gradeThis data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 64.0 J @Temperature 23.0 °C |
47.2 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Lexan® FXE144H PC FXE144H is a Lexan PC Translucent Grade in our VisualFX Portfolio. It is part of Energy family, which includes Illuminate, Glass, and Flame effects. Grade was developed to meet the Aesthetic Differe.. |
|||
Impact Test | 64.0 J @Temperature 23.0 °C |
47.2 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Lexan® FXE144H PC (Asia Pacific) FXE144H is a Lexan PC Translucent Grade in our VisualFX Portfolio. It is part of Energy family, which includes Illuminate, Glass, and Flame effects. Grade was developed to meet the Aesthetic Differe.. |
|||
Impact Test | 64.0 J @Temperature 23.0 °C |
47.2 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Lexan® FXE101R PC Transparent PC. ILLUMINATE special effects (fluorescent/edge glow colors). For thicker sections without sinks. Internal mold release.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 64.0 J @Temperature 23.0 °C |
47.2 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Lexan® FXE101 PC Transparent PC. ILLUMINATE special effects (fluorescent/edge glow colors). 7.0 MFR, for thicker sections without sinks.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 64.0 J @Temperature 23.0 °C |
47.2 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Lexan® FXE144H PC (Europe-Africa-Middle East) FXE144H is a Lexan PC Translucent Grade in our VisualFX Portfolio. It is part of Energy family, which includes Illuminate, Glass, and Flame effects. Grade was developed to meet the Aesthetic Differe.. |