Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 4.89 J | 3.61 ft-lb | Multi-Axial Instrumented Impact Energy; ISO 6603-2 |
LNP Thermotuf® OF-1006 HI Polyphenylene Sulfide, Glass Fiber Reinforcement
(discontinued **) Features: High Impact ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades .. |