Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 3.60 J | 2.66 ft-lb | Multi-Axial Instrumented Impact Energy; ISO 6603-2 |
LNP Konduit® OTF-202-10 Polyphenylene Sulfide, Carbon Fiber Reinforcement
(discontinued **) Features: Electrically Conductive, Thermally ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; h.. |