Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 4.50 J | 3.32 ft-lb | ASTM G14 (modified) |
3M Scotchkote™ 162PWX Epoxy Coating 3M Scotchkote Epoxy Coating 162PWX is a 100% solid two-part epoxy coating that has been specifically developed for the long term protection of drinking water pipelines, storage and process tanks or .. |