Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 26.9 J @Thickness 4.00 mm |
19.8 ft-lb @Thickness 0.157 in |
Multi-axial, at failure; ASTM D3763 |
Azdel AZMET® CM32350 35% continuous random fiber mat / PET resin matrix AZDEL® CM20350 is a glass mat thermoplastic laminate based upon a random oriented continuous fiber mat contained within a Polyethylene Terephthalate (PET) resin matrix. This composite material fea.. |