Polymer Property : Impact Test = 26.6 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 36.0 J

@Temperature 23.0 °C
26.6 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Noryl NH3060 PPE+HIPS
NH3060 resin is a modified PPE + PS blend with an excellent balance of non-chlorinated non-brominated flame retardance, hydrolytic stability, impact and heat resistance, good flow, and low specific ..
Impact Test 36.0 J
26.6 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP STAT-LOY NX13401 PC+ABS
LNP* STAT-LOY* NX13401 is a compound based on PC+ABS blend. Added features of this material include: Antistat, Flame Retardant, Excellent Release.
Impact Test 36.0 J

@Temperature 23.0 °C
26.6 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak; ASTM D 3763
SABIC Innovative Plastics Noryl EM6100F PPE+PS
Automotive interiors. 240F HDT. High impact/good property retention after heat ageing. In blowmolding, better sandability of flash, overblow.This data was supplied by SABIC-IP for the Americas re..