Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 30.5 J @Temperature -40.0 °C |
22.5 ft-lb @Temperature -40.0 °F |
Instrumented, 15 mph; ASTM 3763 |
Phillips Sumika Marlex® CHP-035 Thermoplastic Polyolefin
(discontinued **) Applications: Painted air-bag coversSoft interior trimSoft touch overmoldingInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. |