Impact Test 25.9 J
19.1 ft-lb
Instrumented; ASTM 3763
Chevron Phillips K-Resin® BK18 Styrene-Butadiene Copolymer  (discontinued **)
Characteristics: Good flexibilityGood impact resistanceGood clarityGood mold releaseApplications: ToysOvercapsConsumer productsInformation provided by Chevron Phillips.