Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 25.8 J @Temperature 22.8 °C |
19.0 ft-lb @Temperature 73.0 °F |
Dynatup Instrumented Impact; ASTM D3763 |
Spartech Royalite R86 PVC Acrylic Weather Resistant Sheet Description: Weather Resistant SheetInformation provided by Spartech. |