Polymer Property : Impact Test = 17.5 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 23.7 J

@Thickness 3.17 mm
17.5 ft-lb

@Thickness 0.125 in
Drop Impact, plaques. Fina API test
Total PPR 7425 Polypropylene, Injection Molding Grade
Random copolymer for injection moldingClarity - FINA 7425, a random copolymer, exhibits excellent clarity when molded in polished molds.Impact - FINA 7425 produced molded parts with measurably impro..
Impact Test 23.7 J

@Temperature 23.0 °C
17.5 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Dow AIM® 4900 High Impact Styrenic Resin
AIM® 4900 advanced styrenic resin for extrusion and thermoforming applications is designed to offer the processability of high impact polystyrene and the gloss and practical toughness of high gloss..
Impact Test 23.7 J
17.5 ft-lb
multiaxial, 2.2 m/s; ASTM D3763
Solvay Engineered Polymers DEXFLEX® 925 TPO  (discontinued **)
Description: DEXFLEX® 925 is a thermoplastic olefinic elastomer (TPO) designed for automotive exterior applications that require a combination of stiffness, low-temperature impact resistance, and e..