Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 130.65 J | 96.362 ft-lb | Cum. Energy; Dynatup |
KYDEX® 6503 Integral Pearlescent Low Heat Release Aviation Thermoforming Sheet Features:Thicknesses from 0.71 mm to 3.18 mmChemical resistant - easy to clean with aggressive cleanersForms deep draws with low forces when heated to the upper end of forming temperature rangeCrisp.. |