Mechanical Properties Metric English Comments
Impact Test 18.3 J
13.5 ft-lb
hardness of 62 HRC
Bohler-Uddeholm UDDEHOLM VANADIS 6 Cold Work Tool Steel
Description: Chromium-molybdenum-vanadium alloyed PM steel. Toolmaking with highly alloyed tool steel means that machining and heat treatment have to be considered more than with lower alloyed grade..