Polymer Property : Impact Test = 120 ft-lb
Polymer Property :
Impact Test =
120 ft-lb
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Impact Test
163
J
120
ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Lexan® ML7691 PC
UV stabilized clear polycarbonate formula for internal uses only.