Impact Test >= 102 J
>= 75.0 ft-lb
Intrusion; ASTM D2794
Parker Chomerics CHO-SHIELD® 4994 Conductive Flexible Coating
Description: CHO-SHIELD® 4994 is a smooth, highly conductive flexible silver-filled polyurethane coating designed for military/aerospace airframe applications. Both coatings provide superior adhesi..
Impact Test >= 102 J
>= 75.0 ft-lb
Extrusion; ASTM D2794
Parker Chomerics CHO-SHIELD® 4994 Conductive Flexible Coating
Description: CHO-SHIELD® 4994 is a smooth, highly conductive flexible silver-filled polyurethane coating designed for military/aerospace airframe applications. Both coatings provide superior adhesi..
Impact Test >= 102 J
>= 75.0 ft-lb
Intrusion; ASTM D2794
Parker Chomerics CHO-SHIELD® 4998 Conductive Flexible Coating
Description: CHO-SHIELD® 4998 is a smooth, highly conductive flexible silver-filled polyurethane coating designed for military/aerospace airframe applications. Both coatings provide superior adhesi..
Impact Test >= 102 J
>= 75.0 ft-lb
Extrusion; ASTM D2794
Parker Chomerics CHO-SHIELD® 4998 Conductive Flexible Coating
Description: CHO-SHIELD® 4998 is a smooth, highly conductive flexible silver-filled polyurethane coating designed for military/aerospace airframe applications. Both coatings provide superior adhesi..
Impact Test 102 J
75.2 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP STAT-KON DEL22P PC
LNP STAT-KON* DEL22P is a compound based on Polycarbonate resin containing 10% Carbon Fiber, 10% PTFE. Added features of this material include: Electrically Conductive. Exceptional Processing, Wear..
Impact Test 102 J
75.2 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP STAT-KON DEL22P PC (Asia Pacific)
LNP STAT-KON* DEL22P is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive.