Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 0.790 J | 0.583 ft-lb | unspecified impact test |
Du-Co Ceramics DC-265-L-6 Alumina, 96% Al2O3 Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company. |