Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 0.904 J | 0.667 ft-lb | Instrumented Impact - Energy to Max; Amco Internal Test |
Amco Amalloy® B1044 Polymer Alloy Amco Amalloy B1044 is a proprietary copolymer with exceptional clarity and toughness.Low haze, low melt flow, high tensile & flexural strength.Information provided by Amco Plastic Materials. |