Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 0.580 J | 0.428 ft-lb | unspecified impact test |
Du-Co Ceramics DC-200-L-5 Fosterite Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company. |