Mechanical Properties Metric English Comments
Impact Test 0.750 J
0.553 ft-lb
Dynatest, Penetration Energy; ISO 7765-2
Borealis Borsoft™ SA233CF High Impact Polypropylene Random Heterophasic Copolymer for Blown Film
Borsoft SA233CF is a very soft random heterophasic copolymer, suitable for use on conventional blown film lines with air-coolingBorsoft SA233CF is especially suitable for soft packaging, hygienic fi..