Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Toughness | 432 J | 319 ft-lb | Per square meter |
Hexcel® HexPly® 6376 175°C Curing Epoxy Matrix HexPly® 6376 is a high performance tough matrix formulated for the fabrication of primary aircraft structures. It offers high impact resistance and damage tolerance for a wide range of high tempera.. |