Polymer Property : Toughness = 193 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Toughness 193 J
142 ft-lb
Per square meter; Tested in accordance with EGF Task Group on Polymers and Composites protocol.
Hexcel® HexPly® M18 356°F (180°C) Curing Epoxy Matrix
HexPly® M18 has been developed to fulfill the requirements of the aerospace industry for primary structures using standard manufacturing processes. The matrix has improved properties which allow ea..