Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Toughness | 150 J | 111 ft-lb | Per square meter |
Hexcel® HexPly® 924 180°C Curing Epoxy Matrix HexPly® 924 is a controlled flow epoxy matrix developed for the fabrication of high temperature resistant primary structures. When cured, HexPly® 924 becomes a tough composite with high impact res.. |