Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Toughness | 14.5 J | 10.7 ft-lb | 1.2 pcf density |
NOVA Chemicals Arcel 730 70% PS/30% PE Interpolymer ARCEL is a high-performance, moldable foam resin consisting of 70% polystyrene (PS) and 30% polyethylene (PE). ARCEL provides toughness, flexibility and durability in a lightweight foam.The strength.. |