Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0540 GPa | 7.83 ksi | |
Lubrizol Estane® GP 52 DT Thermoplastic Polyurethane Type: Estane® GP 52DT is an aromatic polyester-based thermoplastic polyurethane (TPU).Features: Translucent spherical pellets.Uses: Injection molding parts, animal identification tagsAvailable in E.. |