Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0434 GPa | 6.30 ksi | ASTM D412 |
Lubrizol Estane® ALR E65D Thermoplastic Polyurethane Type: Estane® ALR E65D is a clear aliphatic thermoplastic polyurethane (TPU).Features: Non-yellowing with good mechanical properties.Available in AmericasInformation Provided by The Lubrizol Corpor.. |