300% Modulus 0.0359 GPa
5.21 ksi
ASTM D412
Lubrizol Estane® 2102-55D Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Load-bearing capacityAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product line from Dow in..