Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0283 GPa | 4.10 ksi | ASTM D412 |
ACC EP RPSP EPI Engineered Polymers Aliphatic Silicone Polymer EP RPSP Aromatic Silicone Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Polyurea with superior performance in industrial applications. EP RPSP displays extremely fa.. |
|||
300% Modulus | 0.0283 GPa | 4.10 ksi | ASTM D412 |
ACC EP RP EPI Engineered Polymers Aromatic Polyurea EP RP, Aromatic Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Polyurea with superior performance in industrial applications. EP RP displays extremely fast cure time.. |