Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0248 GPa | 3.60 ksi | ASTM D412 |
Network Polymers Softflex® 9000 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
300% Modulus | 0.0248 GPa | 3.60 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR N330 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0248 GPa | 3.60 ksi | ASTM D412 |
SK Chemicals SKYTHANE® X595A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
300% Modulus | 0.0248 GPa | 3.60 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR N330 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0248 GPa | 3.60 ksi | ASTM D412 |
Lubrizol Estane® 2103-90A Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Low compression setAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 20.. |
|||
300% Modulus | 0.0248 GPa | 3.60 ksi | ASTM D412 |
Lubrizol Estane® 2355-55DE Thermoplastic Polyurethane Type: Pellethane® 2355-55DE is a thermoplastic polyurethane elastomer.Information Provided by The Lubrizol Corporation |
|||
300% Modulus | 0.0248 GPa | 3.60 ksi | ASTM D412 |
ACC EP LCP EPI Engineered Polymers Aromatic Polyurea EP LCP Aromatic Polyurea, “Powered by Reactamine® Technology” is a two component 100% solid Polyurea (silicone optional) with superior performance in industrial applications. EP LCP displays extr.. |
|||
300% Modulus | 0.0248 GPa | 3.60 ksi | |
Dow Pellethane® 2354-55D Polyurethane Elastomer, Polyester Polycaprolactone Based
(discontinued **) PELLETHANE® 2354-55D is elastomer is a polyester polycaprolactone based polyurethane elastomer used in automotive applications. It allows fast molding, and once molded can be painted with polyureth.. |
|||
300% Modulus | 0.0248 GPa | 3.60 ksi | ASTM D412 |
Dow PELLETHANE® 2355-55DE Polyurethane Elastomer, Polyester Polyadipate Based
(discontinued **) Description: PELLETHANE® 2355-55DE polyester polyadipate based polyurethane elastomer has excellent oil and chemical resistance. Applications include: Film, Sheet, Tubing, Recreation and sporting e.. |