Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0186 - 0.0221 GPa | 2.70 - 3.20 ksi | Secant; Conditioned 7 days at RT/50% RH; ASTM D638 |
AdvanSource Biomaterials ChronoFlex® C 75D Biodurable Medical Grade Polyurethane ChronoFlex® C is a family of premium polycarbonate aromatic biodurable thermoplastic polyurethane elastomers developed by AdvanSource Biomaterials Corporation. ChronoFlex® C medical-grade elastome.. |