Polymer Property : 300% Modulus = 3.13 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.0216 GPa
3.13 ksi
Taiwan Sheen Soon Sheenthane® A9511U Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD.
300% Modulus 0.0216 GPa
3.13 ksi
DIN 53504
Lubrizol ESTANE® 5708F4 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..