Polymer Property : 300% Modulus = 2.47 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.0170 GPa
2.47 ksi
ASTM D412
Lubrizol Advanced Materials PEARLTHANE® 16N92 Thermoplastic Polyurethane Elastomer  (discontinued **)
PEARLTHANE® 16N92 is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent mechanical properties and excellent hydrolysis resistance. It can b..
300% Modulus 0.0170 GPa
2.47 ksi
Injection molded parts; DIN 53504
Huntsman IROGRAN® A 94 E 4900 TPU-Polyester
Introduction: IROGRAN A 94 E 4900 is a thermoplastic polyester polyurethane for melt calendering. IROGRAN is part of the HUNTSMAN technical extrusion/injection molding product range and offers a spe..
300% Modulus 0.0170 GPa
2.47 ksi
ASTM D412
Lubrizol ESTANE® 58132 Ester Based Thermoplastic Polyurethane
Features: Fast cycling, broad temperature performance, and durabilityUses: Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol
300% Modulus 0.0170 GPa
2.47 ksi
Compounded, 35 mins.; ASTM D3185
Dynasol Solprene® 303 Random-Block Copolymer
Solprene 303 is a linear random-block styrene-butadiene copolymer with 46% styrene content, 11% present as a polystyrene block. S-303 is used in vulcanized microcellular shoe soles, it provides hard..