Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0159 GPa | 2.31 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.5 PHR Zinc Stearate Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
300% Modulus | 0.0159 GPa | 2.31 ksi | DIN 53504 |
Huntsman IROGRAN® A 92 P 4637 TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
300% Modulus | 0.0159 GPa | 2.31 ksi | Injection molded parts; DIN 53504 |
Huntsman IROGRAN® A 91 P 4945 TPU-Polyester Introduction: IROGRAN A 91 P 4945 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications. IROGRAN A 91 P 4945 is part of the HUNTSMAN technical ext.. |
|||
300% Modulus | 0.0159 GPa | 2.31 ksi | |
Lubrizol ESTANE® 5708 Ester Based Thermoplastic Polyurethane Features: Very resilient product with excellent resistance to abrasion and tearing, low temperature flexibility, and resistant to certain chemicals.Uses: Hot melt adhesive, synthetic leather and fab.. |
|||
300% Modulus | 0.0159 GPa | 2.31 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.5 PHR Zinc Stearate Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
300% Modulus | 0.0159 GPa | 2.31 ksi | DIN 53504 |
Lubrizol ESTANE® 58563 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |