Mechanical Properties Metric English Comments
300% Modulus 0.0133 GPa
1.93 ksi
Formulation Example; Press Cure 7'/177ºC
TSE Industries Millathane® 28 Millable Polyester Polyurethane Rubber
Millathane 28 has excellent resistance to gas (e.g., nitrogen) permeability as well as very good abrasion resistance and low temperature properties. This polyurethane rubber was designed for automot..
300% Modulus 0.0133 GPa
1.93 ksi
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, Hardness 81A
Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed ..
300% Modulus 0.0133 GPa
1.93 ksi
ASTM D412
Styron Buna® SB 1723 Schkopau Cold Polymerized Emulsion Styrene Butadiene Rubber (E-SBR)
Composition: Buna® SB 1723 – Schkopau is manufactured by cold polymerization using mixed rosin acid /fatty acid soaps. In relation to solid rubber it is plasticized with 37.5 parts of TDAE o..
300% Modulus 0.0133 GPa
1.93 ksi
Formulation Example; Press Cure 7'/177ºC
TSE Industries Millathane® 28 Millable Polyester Polyurethane Rubber
Millathane 28 has excellent resistance to gas (e.g., nitrogen) permeability as well as very good abrasion resistance and low temperature properties. This polyurethane rubber was designed for automot..
300% Modulus 0.0133 GPa
1.93 ksi
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, Hardness 81A
Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed ..