Mechanical Properties Metric English Comments
300% Modulus 0.00730 - 0.0122 GPa
1.06 - 1.77 ksi
Cure: 40 mins at 135°C; ISO 37
Kraton® Cariflex™ IR0310 K Polyisoprene
Description: Cariflex IR0310 KU polymer is a solution polymerized polyisoprene with a high cis-1,4 content. It has a high molecular weight as indicated by its Logarithmic Inherent Viscosity (LIV) va..