Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.01200 GPa | 1.740 ksi | ASTM D412 |
Lubrizol Advanced Materials PEARLCOAT® 165K Thermoplastic Polyurethane Elastomer PEARLCOAT® 165K is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low-temperature flexibility and very good hydrolysis resistance. PE.. |