Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.0119 GPa
1.73 ksi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 3 PHR Di-Cup 40C
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
300% Modulus 0.0119 GPa
1.73 ksi
DIN 53504
Lubrizol ESTANE® T5134 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
300% Modulus 0.0119 GPa
1.73 ksi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 3 PHR Di-Cup 40C
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..