Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0109 GPa | 1.58 ksi | Vulcanized |
KKPC KOSYN 1712H Styrene Butadiene Rubber Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and.. |