Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | >= 0.008798 GPa | >= 1.276 ksi | ZCI-T-008 |
Zeon Chemicals Zetpol® 2000 Hydrogenated Nitrile Elastomomer Zeptol 2000 is a highly saturated copolymer of butadiene and acrylonitrile with high tensile strength, excellent heat resistance, good checmial resistance to aggressive fluids, and an excellent bala.. |