Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.008791 GPa | 1.275 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR Mistron Vapor Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.008791 GPa | 1.275 ksi | ASTM D412 |
SK Chemicals SKYTHANE® S385A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
300% Modulus | 0.008791 GPa | 1.275 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR Mistron Vapor Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |